4.7 Article

Preparation of short CF/GF reinforced PEEK composite filaments and their comprehensive properties evaluation for FDM-3D printing

Journal

COMPOSITES PART B-ENGINEERING
Volume 198, Issue -, Pages -

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.compositesb.2020.108175

Keywords

Fused deposition modeling; Heat-resistant resin; Fiber reinforced PEEK composites; Mechanical properties

Funding

  1. Shandong Science Fund for Distinguished Young Scholars [JQ201715]
  2. National Natural Science Foundation of China [51575322]
  3. Major Program of Shandong Province Natural Science Foundation [ZR2018ZA0401, ZR2018ZB0521]
  4. Key Research and Development Program of Shandong Province [2019GGX104049]
  5. Chinese Scholarship Council (CSC)

Ask authors/readers for more resources

Fused deposition modeling (FDM) has been successfully applied to fabricating short fiber reinforced polymer composites parts. However, due to the intrinsically limited mechanical properties of matrix polymers, there is critical need to develop fiber reinforced high-performance thermoplastic composites for FDM-3D printing to expand engineering applications. In this work, the potential of FDM-3D printing short carbon fiber (CF) and glass fiber (GF) reinforced high-performance PEEK composites has been investigated. Composite filaments with fiber contents of 5 wt%, 10 wt% and 15 wt% were prepared using extrusion process and characterized by micro-morphology observation; and thermal properties testing demonstrated its better thermal stability than pure PEEK. The performance evaluation of printed CF/GF-PEEK parts was focused, including mechanical properties, microstructure, surface quality and porosity. The results indicate that the addition of CF/GF to PEEK can significantly enhance the tensile and flexural strength at the cost of ductility. Lower fiber content of 5 wt% is conducive to increasing mechanical properties, improving surface quality and reducing porosity of printed CF/GF-PEEK. GF/PEEK has better interfacial bonding than CF/PEEK due to the different surface treatments on fibers. Furthermore, microstructure observation suggests that fibers aligned along the printing orientation can strengthen the properties, while pores lead to performance degradation of 3D printed CF/GF-PEEK.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available