4.7 Article

Comparison of performances of early aged pre-vibrated cement-stabilized macadam formed by different compactions

Journal

CONSTRUCTION AND BUILDING MATERIALS
Volume 239, Issue -, Pages -

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.conbuildmat.2019.117682

Keywords

Cement-stabilized macadam; Pre-vibrated; Static; Vibration compaction; Performances

Funding

  1. National Natural Science Foundation of China [51978080]
  2. Joint Fund of the National Natural Science Foundation of China [U1833127]
  3. China Civil Aviation Administration [U1833127]
  4. Nature Science Foundation of Hunan Province [2018114016]
  5. Key Scientific Research Projects of Hunan Education Department [18A129]

Ask authors/readers for more resources

The cement-stabilized macadam formed by static (SC) and vibration compaction (VC) were pre-cracked and their properties comparison were conducted. It indicated that the lowest self-healing rate of VC and SC at 7 days were 57.1% and 54.2%, respectively, with the pre-cracking time of 3 days and degree of 40%. It proved that the shrinkage strains of VC and SC were reduced at most by 35.8% and 35.3%, respectively, with the pre cracking time of 2 days and degree of 40%, respectively, and the corresponding crack resistance were improved by nearly 300%, with the time of 2 days and degree of 30%. The results showed that VC had a better performance. (C) 2019 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available