4.7 Article

Durability of steel fibre-reinforced recycled coarse aggregate concrete

Journal

CONSTRUCTION AND BUILDING MATERIALS
Volume 232, Issue -, Pages -

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.conbuildmat.2019.117119

Keywords

Recycled concrete; Steel fibre; Carbonation resistance; Freeze-thaw cycle; Chloride penetration resistance

Funding

  1. National Natural Science Foundation of China [U1704254]
  2. Program for Innovative Research Team of Education Ministry of China [IRT_16R67]

Ask authors/readers for more resources

Although steel fibre-reinforced recycled coarse aggregate concrete (SFRCAC) is a promising structural material owing to its good mechanical properties and minimal environmental impact, there are uncertainties regarding its durability. Carbonation resistance, freeze-thaw resistance, and chloride ion penetration experiments were performed to evaluate the effects of the recycled coarse aggregate (RCA) and the steel fibres on the durability of SFRCAC. The test results indicated that the durability of SFRCAC was more sensitive to the water-cement ratio than to the RCA replacement ratio. A lower water-cement ratio corresponded to a better durability of the SFRCAC. The compactness of the concrete matrix was the key factor influencing the durability of the SFRCAC. The durability performance of the SFRCAC increased as the volume fraction (V-f) increased from 0% to 1.5% and decreased slightly as V-f increased from 1.5% to 2%. Mass loss of 5% was not a suitable failure criterion for the fast freeze-thaw test of the SFRCAC. It was proven that SFRCAC has good durability and can be successfully applied to structural members with proper mixture design. (C) 2019 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available