JOURNAL OF ALLOYS AND COMPOUNDS
Volume 804, Issue -, Pages 450-456Publisher
ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2019.07.022
Keywords
Cross accumulative roll bonding; Metal matrix composites; E-glass fiber; Peeling test: mechanical properties
Ask authors/readers for more resources
In this research, the structure and mechanical properties of 1050 aluminum strips reinforced with E-glass fibers, processed by the cross accumulative roll bonding (CARB) process, were investigated from microscopic, hardness, tensile and peeling viewpoints. The results indicated that the incorporation of the glass fibers in the Al matrix increases strength and micro-hardness but decreases elongation. In addition, it was realized that some of these fibers are broken and changed to short fibers during the CARB process. The presence of the glass fibers strongly also reduces the bond efficiency of the Al strips, typically from 50% to 5%. To compensate this deleterious effect, it was found that at least 25% should be increased to the normal thickness reduction used in CRAB. (C) 2019 Elsevier B.V. All rights reserved.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available