4.7 Article

Biochar properties and lead(II) adsorption capacity depend on feedstock type, pyrolysis temperature, and steam activation

Journal

CHEMOSPHERE
Volume 231, Issue -, Pages 393-404

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.chemosphere.2019.05.128

Keywords

Adsorption kinetics; Adsorption isotherm; Biochar; Oil sands process water; Optimization

Funding

  1. Canada First Research Excellence Fund
  2. China Scholarship Council
  3. Natural Sciences and Enginerring Research Council of Canada (NSERC) Senior Industrial Research Chair (IRC) in Oil Sands Tailings Water Treatment

Ask authors/readers for more resources

Biochar is a promising material for facilitating the reclamation of oil sands process water (OSPW); however, how biochar properties can be optimized for metal removal from OSPW is not well studied. This study was conducted to determine relationships among feedstock type, pyrolysis condition, biochar property, and lead(II) adsorption capacity to demonstrate the potential use of biochar for metal removal from a synthetic OSPW. Sawdust, canola and wheat straw, and manure pellet were pyrolyzed at 300, 500, and 700 degrees C, with or without steam activation. Increasing pyrolysis temperature increased, with a few exceptions, biochar pH, surface area, and carbon content, but decreased hydrogen and oxygen contents and surface functional groups. Steam activation increased surface area but did not affect other properties. For non-steam-activated biochars, canola and wheat straw biochars produced at 700 degrees C had the highest lead(II) adsorption capacity (Q(max_pb)), at 108 and 109 mg g(-1), respectively. Increasing the pyrolysis temperature increased Q(max_pb) due to increased biochar pH, ash content, and surface area by increasing precipitation, ion exchange, and inner-sphere complexation of lead(II). Steam activation increased lead(II) adsorption capacity for most biochars mainly due to the increased surface area, with the highest Q(max_pb) at 195 mg g(-1) for canola straw biochar pyrolyzed at 700 degrees C with steam activation. The adsorption with time followed a pseudo-second order kinetic model. The results of this study will help select most effective biochars that can be produced from locally available agricultural or forestry byproducts that are optimized for metal removal from synthetic OSPW. (C) 2019 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available