4.8 Article

Evolution of the Solid-Electrolyte Interphase on Carbonaceous Anodes Visualized by Atomic-Resolution Cryogenic Electron Microscopy

Journal

NANO LETTERS
Volume 19, Issue 8, Pages 5140-5148

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/acs.nanolett.9b01515

Keywords

Lithium-ion batteries; transmission electron microscopy; cryogenic electron microscopy; solid-electrolyte interphase; carbon anode

Funding

  1. US Department of Energy, Office of Vehicle Technologies under Extreme Fast Charging program
  2. Ford-Stanford Alliance
  3. Thomas V. Jones Stanford Graduate Fellowship
  4. National_Science Foundation Graduate Research Fellowship [DGE-114747]
  5. Department of Defense (DoD) through the National Defense Science AMP
  6. Engineering Graduate Fellowship (NDSEG)
  7. Intelligence Community Postdoctoral Research Fellowship
  8. National Science Foundation [EGGS-1542152]

Ask authors/readers for more resources

The stability of modern lithium-ion batteries depends critically on an effective solid-welectrolyte interphase (SEI), a passivation layer that forms on the carbonaceous negative electrode as a result of electrolyte reduction. However, a nanoscopic understanding of how the SEI evolves with battery aging remains limited due to the difficulty in characterizing the structural and chemical properties of this sensitive interphase. In this work, we image the SEI on carbon black negative electrodes using cryogenic transmission electron microscopy (cryo-TEM) and track its evolution during cycling. We find that a thin, primarily amorphous SEI nucleates on the first cycle, which further evolves into one of two distinct SEI morphologies upon further cycling: (1) a compact SEI, with a high concentration of inorganic components that effectively passivates the negative electrode; and (2) an extended SEI spanning hundreds of nanometers. This extended SEI grows on particles that lack a compact SEI and consists primarily of alkyl carbonates. The diversity in observed SEI morphologies suggests that SEI growth is a highly heterogeneous process. The simultaneous emergence of these distinct SEI morphologies highlights the necessity of effective passivation by the SEI, as large-scale extended SEI growths negatively impact lithium-ion transport, contribute to capacity loss, and may accelerate battery failure.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available