4.8 Article

Enhanced Interfacial Kinetics and High-Voltage/High-Rate Performance of LiCoO2 Cathode by Controlled Sputter-Coating with a Nanoscale Li4Ti5O12 Ionic Conductor

Journal

ACS APPLIED MATERIALS & INTERFACES
Volume 8, Issue 49, Pages 34123-34131

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/acsami.6b11630

Keywords

surface coating; ionic conductor; LiCoO2; magnetron sputtering; Li4Ti5O12; lithium ion battery

Funding

  1. National Science Foundation of China [11234013, 21473022, 51502032, 21673033, 51603028]
  2. Science and Technology Bureau of Sichuan Province of China [2015HH0033]
  3. Fundamental Research Funds for the Central Universities of China [ZYGX2015J027]
  4. Opening Project of State Key Laboratory of Polymer Materials Engineering (Sichuan Univ.) [SKLPME 2016-4-23]

Ask authors/readers for more resources

The selection and optimization of coating material/approach for electrode materials have been under intensive pursuit to address the high-voltage induced degradation of lithium ion batteries. Herein, we demonstrate an efficient way to enhance the high-voltage electrochemical performance of LiCoO2 cathode by postcoating of its composite electrode with Li4Ti5O12 (LTO) via magnetron sputtering. With a nanoscale (similar to 25 nm) LTO coating, the reversible capacity of LiCoO2 after 60 cycles is significantly increased by 40% (to 170 mAh g(-1)) at room temperature and by 118% (to 139 mAh g(-1)) at 55 degrees C. Meanwhile, the electrode's rate capability is also greatly improved, which should be associated with the high Li+ diffusivity of the LTO surface layer, while the bulk electronic conductivity of the electrode is unaffected. At 12 C, the capacity of the coated electrode reaches 113 mAh g(-1), being 70% larger than that of the uncoated one. The surface interaction between LTO and LiCoO2 is supposed to reduce the space-charge layer at the LiCoO2-electrolyte interface, which makes the Li+ diffusion much easier as evidenced by the largely enhanced diffusion coefficient of the coated electrode (an order of magnitude improvement). In addition, the LTO coating layer, which is electrochemically and structurally stable in the applied potential range, plays the role of a passivation layer or an artificial and friendly solid electrolyte interface (SEI) layer on the electrode surface. Such protection is able to impede propagation of the in situ formed irreversible SEI and thus guarantee a high initial columbic efficiency and superior cycling stability at high voltage.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available