Journal
TRIBOLOGY INTERNATIONAL
Volume 61, Issue -, Pages 214-223Publisher
ELSEVIER SCI LTD
DOI: 10.1016/j.triboint.2013.01.003
Keywords
Dry sliding; Oxidative; Wear behavior; Tribo-oxides
Categories
Funding
- National Natural Science Foundation of China [51071078]
Ask authors/readers for more resources
Dry sliding tests were performed for 45, 4Cr5MoSiV1 steels and 3Cr3Mo2V cast steel at 200 and 400 degrees C. The wears at 200 and 400 degrees C are of oxidative wear characteristic due to tribo-oxides formed on worn surfaces. However, the wear at 200 degrees C presents different wear behaviors and characteristics from the one at 400 degrees C. The wear at 200 degrees C is a typical oxidative mild wear, but the wear at 400 degrees C is beyond oxidative mild wear, here called oxidative wear. The characteristics of oxidative mild wear and oxidative wear were clarified. (C) 2013 Elsevier Ltd. All rights reserved.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available