Octaphenylsilsesquioxane (PH-POSS) and octa(?-methacryloxypropyl)silsesquioxane (MA-POSS) were successfully synthesized by hydrolytic condensation of phenyltrichlorosilane and ?-methacryloxypropyltrimethoxysilane, and characterized by Fourier transform infrared (FT-IR), 1H and 29Si nuclear magnetic resonance (NMR), and matrix-assisted laser desorption/ionization-time of flight (MALDI-TOF) mass spectrum. Morphology, degradation behavior, thermal, and mechanical properties of hybrid composites were studied by transmission electron microscopy (TEM), polarized optical microscopy (POM), differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), surface contact angle (SCA), tensile, and impact testing. Domains of PH-POSS and MA-POSS dispersed in the matrix with a wide size distribution in a range of 0.10.5 mu m, while PH-POSS exhibited a preferential dispersion. Because of the possible homopolymerization of MA-POSS during the melt blending, the glass transition temperature of polycarbonate (PC)/MA-POSS composites remained nearly unchanged with respect to PC/PH-POSS composites that showed a depression of Tg due to the plasticization effect. It is interesting to note that the incorporation of POSS retarded the degradation rates of PC composites and thus significantly improved the thermal stabilities. Si O fractions left during POSS degradations were a key factor governing the formation of a gel network layer on the exterior surface. This layer possessed more compact structures, higher thermal stabilities, and some thermal insulation. In addition, percentage residues at 700 degrees C (C700) significantly increased from 10.8% to 15.822.1% in air. Fracture stress of two composites showed a slight improvement, and the impact strength of them decreased monotonically with the increase of POSS loading. Copyright (C) 2011 John Wiley & Sons, Ltd.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available