4.7 Article

Electrospun poly (butylene succinate)/cellulose nanocrystals bio-nanocomposite scaffolds for tissue engineering: Preparation, characterization and in vitro evaluation

Journal

POLYMER TESTING
Volume 71, Issue -, Pages 101-109

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.polymertesting.2018.08.027

Keywords

Electrospinning; Poly (butylene succinate); Cellulose nanocrystals (CNC); Nanocomposite; Scaffolds

Funding

  1. National Natural Science Foundation of China [51803062, 51573063]
  2. Science and Technology Program of Guangzhou [201804010110]
  3. National Postdoctoral Program for Innovation Talents [BX201700079]
  4. China Postdoctoral Science Foundation [2017M620371]
  5. Foundation for Distinguished Young Talents in Higher Education of Guangdong Province [2017KQNCX001]
  6. Guangdong Science and Technology Planning Project [2014B010104004, 2013B090600126]
  7. Open Funding Project of the State Key Laboratory of Bioreactor Engineering of Ministry of Education
  8. Opening Project of Key Laboratory for Ultrafine Materials of Ministry of Education [2017CX001]

Ask authors/readers for more resources

Three-dimensional (3D) bio-nanocomposite poly (butylene succinate) (PBS)/cellulose nanocrystals (CNC) scaffolds were fabricated by a solvent mixture of chloroform (CF) and methanol (MeOH) via electrospinning technique. Morphological, thermal, mechanical, and hydrophilicity as well as in vitro degradation and biocompatibility properties of the electrospun fibrous bio-nanocomposite scaffolds were investigated. Scanning electron microscopy (SEM) indicated that the average diameter of the electrospun fibers decreased with increase in CNC concentration. The incorporation of CNC not only enhanced the thermostability, and 0.5 wt% and 1 wt% CNC significantly increased the crystallinity of PBS matrix, but also improved the tensile strength, Young's modulus and hydrophilicity of PBS matrix with an optimum 3 wt% CNC. Moreover, it also improved the porosity and decreased the density of the PBS/CNC scaffolds. In vitro degradation results showed that PBS/CNC3 scaffold had better bio-degradation ability, from 4.5% of neat PBS to 13.74% of PBS/CNC3 in 28 days. 3T3 fibroblast cell culture was performed to confirm the good biocompatibility of the scaffolds. Cells were found to proliferate better on the PBS/CNC3 scaffolds, as compared to neat PBS scaffolds in 7 days.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available