4.7 Article

Modification of MOR by desilication treatments: Structural, textural and acidic characterization

Journal

MICROPOROUS AND MESOPOROUS MATERIALS
Volume 131, Issue 1-3, Pages 350-357

Publisher

ELSEVIER
DOI: 10.1016/j.micromeso.2010.01.013

Keywords

Mesoporous mordenite; Desilication; FTIR; Al-27 and Si-29 MAS-NMR; Acidity

Ask authors/readers for more resources

The effect of several desilication experimental parameters (base concentration, temperature and time) on the characteristics of MOR zeolite was studied. The samples were characterized by X-ray diffraction, Al-27 and Si-29 MAS-NMR, chemical analysis, and FTIR (framework vibration region). The textural characterization was made by N-2 adsorption and the acidity was evaluated by pyridine adsorption followed by FTIR and by the catalytic model reaction of n-heptane cracking. The alkaline treatments promoted the Si extraction from the zeolite framework, without considerable loss of crystallinity and, as it was envisaged, an important increase of the mesoporous structure was attained. A linear correlation between the number of framework Si per unit cell. N-Si and the asymmetric stretching wavenumber, nu(i), was observed. The acidity characterization shows that the desilicated samples exhibit practically the same acid properties than the parent HMOR zeolite. The optimum desilication conditions were those used to obtain sample M/0.2/85/2, i.e., sample treated with 0.2 M NaOH solution at 85 degrees C for 2 h. (C) 2010 Elsevier Inc. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available