4.3 Article

Dissimilar Metal Joining of 2024 and 7075 Aluminium Alloys to Titanium Alloys by Friction Stir Welding

Journal

MATERIALS TRANSACTIONS
Volume 52, Issue 5, Pages 948-952

Publisher

JAPAN INST METALS & MATERIALS
DOI: 10.2320/matertrans.L-MZ201102

Keywords

friction stir welding; dissimilar metal joining; aluminum alloy; titanium alloy; intermetallic compound

Ask authors/readers for more resources

The friction stir welding (FSW) process is a solid-state joining process and the joining temperature is lower than that used in the fusion welding processes. Therefore, for dissimilar metal welding, FSW is considered to offer several advantages over fusion welding. The present work investigated the weldability of duralumin and titanium alloys using friction stir welding. The aluminum plates used in this work were 2024-T3 and 7075-T651, and the titanium plates used were pure titanium and Ti-6Al-4V. The average tensile strength of the Ti/2024 FSW joints was 311 MPa, and the tensile strength of the Ti/2024 joint was higher than that of the Ti/7075 FSW joint when the joining conditions were the same. A mixed region of Ti alloy and Al alloy was observed at the joint interface, and the joints mainly fractured at this region, where there was an intermetallic compound layer. In this region, a TiAl3 intermetallic compound was detected by XRD. Therefore, it can be understood that this TiAl3 intermetallic compound affects the tensile strength of butt joints. [doi:10.2320/matertrans.L-MZ201102]

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.3
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available