4.7 Article

Microstructure and mechanical properties of AISI 347 stainless steel/A335 low alloy steel dissimilar joint produced by gas tungsten arc welding

Journal

MATERIALS & DESIGN
Volume 50, Issue -, Pages 566-573

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2013.03.029

Keywords

Dissimilar welding; Austenitic stainless steel; Low alloy steels; Microstructures; Mechanical properties

Ask authors/readers for more resources

In the present study, microstructure and mechanical properties of AISI 347 austenitic stainless steel/ASTM A335 low alloy steel dissimilar joint were investigated. For this purpose, two filler metals including ER309L and ERNiCr-3 were selected to be used during the gas tungsten arc welding process. In tension tests, all weldments failed in the HAZ of A335. The impact test results indicated that all specimens exhibited ductile fracture. The maximum fracture energy was related to the ERNiCr-3 weld metal specimen. The maximum and minimum hardness corresponded to the ERNICr-3 and ER309L. Finally, it was concluded that ERNiCr-3 filler metal was the best choice for the joint between 347 austenitic stainless steel and A335 low alloy steel. (c) 2013 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available