Tensile behaviours of quartz, aramid and glass filaments after NaCl treatment

Journal

MATERIALS & DESIGN
Volume 30, Issue 3, Pages 867-870

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2008.05.055

Keywords

Fibres and filaments (B); Corrosion (E); Chemical reactions (F)

Funding

  1. Key Laboratory of China Education Ministry, Zhejiang University of Sciences [2005003]

Ask authors/readers for more resources

Quartz, aramid and glass filaments were treated with NaCl solutions of various concentrations for different periods of time. The appearance of the treated filaments was examined. It revealed that for the quartz fibre the NaCl density and the treatment time have a minor effect as far as the decrease rate of the fibre strength is concerned. After three weeks of NaCl treatment, dramatic degradation of the aramid filaments was noticed for all the NaCl densities used in the investigation. The glass fibre degradation induced by the NaCl solution was considered regular; both higher NaCl concentration and prolonged treating time would both promote the decrease of the fibre strength. (C) 2008 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available