Hydrogen uptake was measured for platinum doped superactivated carbon at 296 K where hydrogen spillover was expected to occur. High pressure adsorption measurements using a Sieverts apparatus did not show an increase in gravimetric storage capacity over the unmodified superactivated carbon. Measurements of small samples (similar to 0.2 g) over long equilibration times, consistent with the reported procedure, showed significant scatter and were not well above instrument background. In larger samples (similar to 3 g), the hydrogen uptake was significantly above background but did not show enhancement due to spillover; total uptake scaled with the available surface area of the superactivated carbon. Any hydrogen spillover sorption was thus below the detection limit of standard volumetric gas adsorption measurements. Due to the additional mass of the catalyst nanoparticles and decreased surface area in the platinum doped system, the net effect of spillover sorption is detrimental for gravimetric density of hydrogen.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available