Use of Heat-Treated Water Treatment Residuals in Fly Ash-Based Geopolymers

Journal

JOURNAL OF THE AMERICAN CERAMIC SOCIETY
Volume 93, Issue 1, Pages 272-278

Publisher

WILEY
DOI: 10.1111/j.1551-2916.2009.03331.x

Keywords

-

Funding

  1. National Basic Research Program (973) of China [(2009CB623100]
  2. China Scholarship Council
  3. School of Environment and Natural Resources, The Ohio Agricultural Research and Development Center, The Ohio State University. Wooster, OH, USA

Ask authors/readers for more resources

Geopolymerization is a developing field that can beneficially use heat-treated water treatment residuals (WTRs) to create fly ash-based geopolymers. In this study, geopolymers made only from fly ash (FA) and from FA plus calcined WTRs (FA-WTRs) were evaluated. The proper calcining condition for WTRs is 900 degrees C for 1 h and the optimum amount of WTRs to mix with FA is 10 wt%. Compressive strength of samples cured at 75 degrees C for 24 h can reach 68.1 MPa, and when cured at 23 degrees C for 28 days the values were >50 MPa. Further studies were conducted on FA and FA-WTRs geopolymer samples cured at 75 degrees C for 8 h followed by 23 degrees C for 28 d. X-ray diffraction patterns of geopolymers made from FA indicate the presence of amorphous geopolymeric and calcium silicate hydrate (C-S-H) gels, and a type of zoelite similar to gismondine. When WTRs replaced some of the FA, amorphous geopolymeric gels are mainly formed. Scanning electron micrographs indicate spherical unreactivated FA and other particles are combined and surround the geopolymeric and C-S-H gels. Utilization of WTRs in creation of FA-based geopolymers can lead to a new type of cementitious binder.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available