Journal
JOURNAL OF SUPERHARD MATERIALS
Volume 30, Issue 5, Pages 297-304Publisher
SPRINGER
DOI: 10.3103/S1063457608050031
Keywords
detonation nanodiamonds; chemical purification; nitric acid; pressure; autoclave; titanium
Categories
Ask authors/readers for more resources
The paper addresses the chemical purification behavior of detonation nanodiamond soot in the case of using a dilute nitric acid under pressure. The optimal process is found to proceed at 230-240C, 7-8 MPa, with HNO3 excess of 200-300% of stoichiometry.