Optimization of SOFC anode/electrolyte assembly based on BaIn0.3Ti0.7O2.85 (BIT07)/Ni-BIT07 using an interfacial anodic layer

Journal

JOURNAL OF POWER SOURCES
Volume 251, Issue -, Pages 66-74

Publisher

ELSEVIER
DOI: 10.1016/j.jpowsour.2013.11.026

Keywords

BaIn0.3Ti0.7O2.85(BIT07)(BIT07) for SOFC; Anode active layer; Ni current collector; Tape casting; Co-sintering; EIS

Ask authors/readers for more resources

BaIn0.3Ti0.7O2.85 (BIT07) is a potential electrolyte material for Solid Oxide Fuel Cells (SOFCs) due to its high ionic conductivity and its compatibility with commonly used cathode materials. By using tape casting and co-sintering shaping methods symmetrical cells BIT07-Ni/BIT07/BIT07-Ni have been prepared. In order to improve the interface between BIT07-Ni and BIT07, a thin anode functional active layer (AAL) deposited between the BIT07-Ni and BITO7 is used. The effect of this layer on the electrochemical performance of the symmetrical cells as well as the influence of an additional Ni current collecting layer deposited on the anode side are discussed in this study. It is shown that the presence of the AAL decreases the area specific resistance (ASR) of the anode/assembly by a factor of about two, and that the presence of the Ni layer slows down the ageing of the assembly. (C) 2013 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available