The photocatalytic activity of 1.0 wt% PdO supported on Al2O3-Nd2O3 binary oxides prepared by the sol-gel method was studied in the photodegradation of 2,4-dichlorophenoxyacetic acid (2,4-D). The photocatalysts were characterized by N-2 physisorption, XRD and UV-vis spectroscopy. MO supported on gamma-Al2O3 photo-degrades the 2,4-D, however the addition of Nd2O3 to gamma-Al2O3 notably improves the photocatalytic activity. As the concentration of Nd2O3 in the binary oxide increases from 2 to 10 wt%, the photodegradation of 2,4-D is highly enhanced. The catalytic test for PdO supported on pure Nd2O3 showed scarce photocatalytic activity. Total organic carbon (TOC) analysis showed that the 2,4-D has been completely destroyed on the PdO/Al2O3-Nd2O3 photocatalysts after 6 h under irradiation. (C) 2011 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available