4.7 Article

Oxidation behavior of ferritic-martensitic and ODS steels in supercritical water

Journal

JOURNAL OF NUCLEAR MATERIALS
Volume 424, Issue 1-3, Pages 261-276

Publisher

ELSEVIER
DOI: 10.1016/j.jnucmat.2012.03.009

Keywords

-

Funding

  1. Pennsylvania State University Materials Research Institute Nanofabrication Lab
  2. National Science Foundation [0335765]
  3. National Nanotechnology Infrastructure Network
  4. DOE-NERI [DE-FC07-06ID14744]
  5. DOE, Basic Energy Sciences, Office of Science [W-31-109-Eng-38]
  6. Cornell University

Ask authors/readers for more resources

Ferritic-martensitic and ODS alloys are primary candidates for application as cladding and structural materials in the Generation IV Supercritical Water Reactor. One of the main in-service degradation mechanisms for these alloys is uniform corrosion. This article analyzes the oxide microstructure formed on these alloys to better understand their oxidation behavior. Corrosion tests were performed in both steam and supercritical water (SCW) at 500 and 600 degrees C. The oxide microstructure was analyzed using microbeam synchrotron radiation diffraction and fluorescence associated with electron microscopy. The oxide forms a three-layer structure with an outer layer containing only Fe3O4, an inner layer containing a non-uniform (Fe,Cr)(3)O-4 spinel structure, and a diffusion layer containing a mixture of metal grains and chromium-rich precipitates. A marker experiment located the original water-metal interface as the outer-inner layer interface implying a mechanism where iron migrates outwards to form the outer layer and oxygen diffuses inwards to form the inner layer. (C) 2012 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available