Hydrothermal processing of MSWI Fly Ash-towards new stable minerals and fixation of heavy metals

Journal

JOURNAL OF HAZARDOUS MATERIALS
Volume 167, Issue 1-3, Pages 250-259

Publisher

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jhazmat.2008.12.119

Keywords

Hydrothermal processing; MSWI fly ash; Tobermorite; Chemical stability

Funding

  1. XRD laboratory

Ask authors/readers for more resources

A hydrothermal processing strategy of MSWI fly ash is presented for obtaining stable minerals with low toxic potential. Different hydrothermal conditions were tested to obtain high yields of new stable minerals. Experimental parameters including temperature, nature and molarity of alkali reagents, and reaction time were evaluated. The chemical stability of hydrothermal products was examined by the toxicity characteristic leaching procedure (TCLP) test and subsequent XRD for the leached residue. The significant amounts of Al-substituted 11 angstrom tobermorite and katoite in addition to minor amounts of zeolites were formed under experimental conditions at 0.5 M NaOH, 180 degrees C for 48 h, however KOH treatment in a similar regime resulted in smaller amounts of Al-substituted 11 angstrom tobermorite and katoite. Similarly, a product of mixed Al-substituted 11 angstrom tobermorite and katoite could be formed from the washed fly ash treated in 0.5 M NaOH at 180 degrees C for 48 h. Under the acidic condition, the treated fly ash exhibited an excellent stability of the mineral assemblage and less release of heavy metals relative to the untreated parent materials. (C) 2008 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available