Ni/CeO2-Al2O3; Dry reforming; Nickel particle size; CeAlO3; Carbon deposition
Categories
Ask authors/readers for more resources
The catalytic performances of Ni/CeO2-Al2O3 catalysts for the dry reforming of CH4 (DRM) were investigated. Catalysts with different Ni dispersion and different amount of CeAlO3 species were prepared by different methods and characterized by BET, XRD, XPS, Raman, TPR and TPO techniques. Catalytic activity was studied during time on stream in the range 873-1073 K with a mixture of CH4:CO2:Ar = 40:40:20 vol.% and GHSV 90,000 cm(3) g(-1) h(-1). The intrinsic catalytic activity increased with the increasing of Ni crystallite size. Carbon was deposited as nano-fibres and graphite when catalysts worked at lower temperature, and the largest amount was found on the catalyst with the largest Ni crystallite size. The formation of graphitic deposits is limited by the presence of CeAlO3 species formed during catalyst activation. CA preparation method results particularly attractive because it allows to obtain catalysts with small Ni crystallite size and high content of CeAlO3 species, which both have a role in suppressing the carbon deposition and therefore in obtaining stable catalytic performances. (C) 2015 Elsevier B.V. All rights reserved.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available