4.6 Article

Long-term evaluation of water sorption and ultimate tensile strength of HEMA-containing/-free one-step self-etch adhesives

Journal

JOURNAL OF DENTISTRY
Volume 39, Issue 7, Pages 506-512

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.jdent.2011.04.008

Keywords

One-step self-etch adhesives; Polymers; Ultimate tensile strength; Water sorption; HEMA

Funding

  1. Japanese Ministry of Education, Global Center of Excellence (GCOE) Program, International Research Center for Molecular Science in Tooth and Bone Diseases
  2. Grants-in-Aid for Scientific Research [23792165] Funding Source: KAKEN

Ask authors/readers for more resources

Objective: The objective of this study was to evaluate the water sorption (Wsp) and ultimate tensile strength (UTS) of HEMA-containing/free one-step self-etch adhesives after long-term water-storage. Methods: Three HEMA-containing one-step self-etch adhesives (Bond Force (BF), Clearfil S(3) Bond (S3) and OptiBond All-In-One (OP)), and one HEMA-free one-step self-etch adhesive, G Bond (GB) was used. After the solvents of each adhesive were evaporated, polymerised adhesive disks and dumbbell-shaped specimens of thirty-two each were prepared and divided into four groups of 14-, 90-, 180- and 360-day water-storage. After immersion in water for the designated storage periods, the disks were subjected to measurement of Wsp, and the dumbbell-shaped specimens were subjected to measurement of UTS. The data of Wsp and UTS were statistically analysed using a two-way ANOVA and Bonferroni test. Results: Wsp of BF, S3 and OP increased over time, whereas for GB, there were no significant differences in Wsp among all the storage periods. Wsp of GB was lower than those of BF, S3 and OP in each period. The UTS of BF, S3 and OP decreased over time, whereas for GB, there were no significant differences in UTS among all storage periods. The highest UTS was initially seen in BF > GB = S3 = OP, and after 360-day water-storage, seen in BF = GB > OP = S3. Conclusions: For the HEMA-containing adhesives, Wsp increased and UTS decreased over time. On the other hand, for the HEMA-free adhesive, Wsp and UTS did not significantly change even after 360-day water-storage. (C) 2011 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available