JOURNAL OF COMPOSITE MATERIALS
Volume 42, Issue 25, Pages 2673-2685Publisher
SAGE PUBLICATIONS LTD
DOI: 10.1177/0021998308096329
Keywords
polymer-matrix composite; mechanical properties; hardness; thermal properties
Categories
Funding
- Ministry of Education and Research [X2C29]
Ask authors/readers for more resources
A series of cork and black carbon filler incorporated cross-linked molded polyurethane (PU), based on polyethylene adipate diol and 4,40 diphenyl methane diisocyanate with 1,4 butane diol or 1,6 hexane diol and glycerin as chain extender, were synthesized. Mechanical properties were examined in composites that had between 1 and 15% cork and carbon black between 2 and 3%. Therefore, in order to understand the behavior of fillers, such as carbon black and cork added to cross-link polyurethane resins, several thermal and mechanical tests were conducted on samples, made of these new materials. The mechanical properties of the composites were found to depend mostly on the type and amount of filler. The results show that the polyurethane component ratios in cross-linked polymers, the types of filler, and the amount of powder added all affect the properties of the filled cross-linked polyurethanes. The addition of cork filler into polyurethane composites yields an increase in Young's modulus and a decrease in the elongation at break. This new cross-linked polyurethane-matrix and polyurethane-cork composite materials with better damping properties can be used as a bearing pad for acoustic and vibratory isolation for railway and underground lines.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available