4.8 Article

Cobalt particle size effects on catalytic performance for ethanol steam reforming - Smaller is better

Journal

JOURNAL OF CATALYSIS
Volume 318, Issue -, Pages 67-74

Publisher

ACADEMIC PRESS INC ELSEVIER SCIENCE
DOI: 10.1016/j.jcat.2014.07.020

Keywords

Steam reforming of ethanol; Cobalt on carbon nanofibers (Co/CNF); Cobalt particle size effects; Catalyst stability; Coke formation

Funding

  1. Shell Global Solutions
  2. [CTENERG/FINEP-01.04.0525.00]

Ask authors/readers for more resources

The effect of the cobalt particle size in the ethanol steam reforming reaction at 773 K for hydrogen production was investigated using cobalt on carbon nanofiber catalysts. It was found that the turnover frequency increases with decreasing Co particle size, which was attributed to the increasing fraction of edge and corner surface sites with decreasing size. Regarding catalyst stability, a decrease in deactivation rate was observed with decreasing cobalt particle size. This was caused by a significantly lower amount of carbon deposition on the smallest Co particles than on larger ones, as concluded from transmission electron microscopy measurements. The reduced amount of carbon deposition is ascribed to a lower fraction of terrace atoms, proposed to be responsible for initiation of carbon deposition on catalysts with large (>10 nm) Co particles. Therefore, it was concluded for this non-noble metal that the smallest particles perform best in catalysis of ethanol steam reforming. (C) 2014 Elsevier Inc. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available