JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS
Volume 93B, Issue 2, Pages 468-475Publisher
WILEY
DOI: 10.1002/jbm.b.31604
Keywords
adhesion; UHMWPE; TiN coating; oxidized zirconium; transfer layer
Ask authors/readers for more resources
The classical wear mechanisms abrasion, fatigue, and adhesion are the most frequent causes of surface changes of ultra high molecular weight polyethylene (UHMWPE) in artificial joints The counterpart material has a strong influence on the wear and friction behavior of artificial Joints due to its abrasive properties and adhesive interaction with UHMWPE The formation of a transfer layer on the counterpart in UHMWPE bearing systems is often described as being a clear indication of strong adhesive forces The influence of using a cobalt-chromium-molybdenum (CoCrMo) alloy, a titanium nitride plasma coating or an oxidized zirconium alloy on adhesive wear was studied The surface free energy and the bonding forces of these counterpart materials to UHMWPE were investigated Catalytic effects on the degradation behavior of polyethylene, the micro friction behavior, and the build-up and constitution of a transfer layer deposited under loads, and relative velocities that are relevant in knee joints were analyzed (C) 2010 Wiley Periodicals, Inc J Biomed Mater Res Part B Appl Biomater 938 468-475, 2010
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available