4.6 Article

Constitutive modeling of biodegradable polymers: Hydrolytic degradation and time-dependent behavior

Journal

INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES
Volume 51, Issue 5, Pages 1164-1174

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.ijsolstr.2013.12.010

Keywords

Constitutive models; Time-dependent behavior; Biodegradable polymers; Functional compatibility

Categories

Funding

  1. CAPES/CNPq [022/2012]
  2. Program USP/UP
  3. FCT (Portuguese Science and Technology Foundation) [PTDC/EME-PME/114808/2009]
  4. Fundação para a Ciência e a Tecnologia [PTDC/EME-PME/114808/2009] Funding Source: FCT

Ask authors/readers for more resources

A large range of biodegradable polymers has been used to produce implantable medical devices. Apart from biological compatibility, these devices shall be also functional compatible and perform adequate mechanical temporary support during the healing process. However, the mechanical behavior of biodegradable materials during its degradation, which is an important aspect of the design of these biodegradable devices, is still an unexplored subject. Based on the literature, the mechanical behavior of biodegradable polymers is strain rate dependent and exhibits hysteresis upon cyclic loading. On the other hand, ductility, toughness and strength of the material decay during hydrolytic degradation. In this work, it is considered a three-dimensional time-dependent model adapted from the one developed by Bergstrom and Boyce to simulate the performance of biodegradable structures undergoing large deformations incorporating the hydrolysis degradation. Since this model assumes that the mechanical behavior is divided into a time independent network and a non-linear time-dependent network, it enables to simulate the monotonic tests of a biodegradable structure loaded under different strain rates. The hysteresis effects during unloading-reloading cycles at different strain levels can be predicted by the model. A parametric study of the material model parameters evolution during the hydrolytic degradation was conducted to identify which parameters are more sensible to this degradation process. The investigated model could predict very well the experimental results of a blend of polylactic acid and polycaprolactone (PLA-PCL) in the full range of strains until rupture during hydrolytic degradation. From these results and analyses, a method is proposed to simulate the three-dimensional mechanical behavior during hydrolytic degradation. (C) 2013 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available