4.7 Article

Degradation mechanism of electrolyte and air electrode in solid oxide electrolysis cells operating at high polarization

Journal

INTERNATIONAL JOURNAL OF HYDROGEN ENERGY
Volume 38, Issue 3, Pages 1225-1235

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.ijhydene.2012.10.113

Keywords

Solid oxide electrolyzer; Impedance spectroscopy; Anodic current; Degradation; Densification

Funding

  1. institutional research program of the Korea Institute of Science and Technology [2E22802]
  2. Manpower Development Program for Energy of the Ministry of Knowledge and Economy (MKE), Republic of Korea
  3. Korea Evaluation Institute of Industrial Technology (KEIT) [20094020200010] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

Degradation mechanism of the electrolyte and air electrode is reported for solid oxide electrolysis cells (SOECs). Symmetric cells composed of yttria-stabilized zirconia (YSZ) electrolyte, Sr-doped LaMnO3 +/-delta (LSM)/YSZ composite working and counter electrodes, and Pt ring-type reference electrode are used to simulate the operating conditions of the air electrode. Degradation behavior in the impedance spectra is characterized as growth of mid-frequency arc at the initial stage, gradual increase of ohmic resistance throughout the operation, and sharp rise of low frequency resistance at the final stage, followed by catastrophic cell failure. Initial stage degradation is attributed to deactivation of LSM, resulting from reduction of oxygen vacancy concentration and/or segregation of passivation species on LSM surface under anodic current passage. Intergranular fracture, which occurs along the grain boundaries of the YSZ electrolyte, is responsible for gradual increase of ohmic resistance. Increase of low frequency arc at the final stage is caused by densification of the air electrode, leading to excessive pressure build-up and delamination of the air electrode. Cation migration, which is facilitated by oxygen excess nonstoichiometry of LSM and externally applied electric field, is considered to be the main cause of permanent damages. Copyright (C) 2012, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available